Three coverings built three different ways
A flat roof covering has one job, which is to keep water out of a roof that has only a slight fall. EPDM, GRP and felt all do that job, but they are made differently, laid differently and repaired differently, and a choice between them is a choice between those methods as much as between materials.
EPDM is a rubber sheet that arrives in a roll, cut to size and fixed to the deck. GRP is glass-reinforced plastic, a fibreglass laminate built up on the roof in resin and finished with a topcoat, which sets into one continuous surface. Felt is bitumen-based sheeting, laid in layers and joined by heat or adhesive. Of the three, EPDM alone belongs to the single-ply group, so when a quote describes a GRP or felt roof as single-ply, the word has been used loosely.
| Covering | Form | Joined by |
|---|---|---|
| EPDM | Rubber sheet | Adhesive or tape |
| GRP | Resin and glass fibre | Cured as one surface |
| Felt | Bitumen layers | Heat or adhesive |
The flat roofing page covers the wider choice of flat roof coverings, from garage roofs to extensions and porches. TPO is a second single-ply material, laid on larger buildings, and it belongs to the commercial roofing section of this site. Beyond how each is made, the three differ in published lifespan, in price and in the checks that decide between them on a given roof.
EPDM: the rubber sheet
EPDM is synthetic rubber, and a garage or extension roof can be covered with a single sheet cut to the size of the roof, so there are no seams across the main area. The sheet is bonded to the deck or insulation with adhesive, then folded up at the edges and finished with moulded corners and trims. Where two pieces meet, a seam is made with adhesive or jointing tape.
Because the sheet comes in one piece, the quality of the surface beneath shows through. The deck has to be sound, dry and smooth, with no sharp edges, since the rubber is thin and a screw head or a loose splinter can mark it. New boards are laid first if the old deck is not fit to take a covering.
EPDM can be cut and patched if it is damaged. The repair is made with the manufacturer's adhesive and patch material, to a clean, dry surface. A patch of the wrong product can lift and let water in again, so the existing material is identified before anything is stuck to it.
The details around the sheet decide how well it performs: upstands at the wall, edge trims, outlets and any rooflight kerbs. These are formed on site and carry as much weight as the main sheet, because a roof leaks at a detail more readily than across an open field of membrane.
GRP: fibreglass laid wet
GRP is built on the roof. A deck is prepared, a layer of resin is rolled on, and glass-fibre matting is laid into it and worked until the fibres are saturated. Once it cures, a top coat is applied. The result is a hard, continuous surface without the joints that a roll of sheeting has, which is the main reason people consider it for roofs with awkward shapes and many corners.
Trims at the edges, called drip trims or edge trims, are fitted before the resin goes on, and the resin forms around them as a sealed part of the surface. Upstands at walls are formed in the same laminate, so the roof and its upturns are one piece.
The deck beneath must be stiff, because a hard laminate will crack if the boards move under it. Timber needs to be dry and well fixed, and resin has to cure in suitable weather: it does not set properly on a wet deck or in the damp. A mild, dry spell suits the work.
A GRP roof is repaired by cleaning back the damaged area, laying new laminate and finishing it with a topcoat. A repair matched to the surrounding colour and finish is possible, but the patch has to bond to old resin, which needs the old surface to be prepared.
Felt: bitumen laid in layers
Built-up felt is made of a base layer and a cap sheet of bitumen-coated material. The layers are bonded together and to the deck, either by torch, with a gas flame softening the underside of the sheet, or with cold-applied adhesive. Torch-on felt is the name Less uses for the hot-bonded type. Joints between rolls overlap and are sealed as the layers go down.
Felt has a long history on flat roofs, and its basic principle is layering: if one layer is breached, the others still shed water. That is the idea behind specifying two or three layers instead of one, and the number of layers in a quote tells you what is being offered.
Felt products differ in quality, and the published lifespans are given as ranges. The cap sheet, the base and the care taken with laps, edges and upstands all affect how a felt roof wears. A hot-bonded roof also needs a careful assessment of the site, because a naked flame on a roof close to combustible materials carries a fire risk, which the contractor must plan for.
Felt repairs are made by cutting out the failed area and patching it with new sheet, laid to overlap the surrounding roof and bonded to it. Small splits and blisters can be dealt with this way, though a roof with failure across its width needs more than a patch.
What two sources say about lifespan
Two published sources give lifespans for these coverings, and their figures differ. HomeBuilding's numbers are approximate and carry a last-updated date of 30 September 2025. Less publishes its own ranges, on a page it last updated on 12 November 2026. The table sets them out in two columns, one for each source, with the covering down the side. Read down a column to see how one source ranks the three, and across a row to see where the two sources sit side by side.
| Covering | HomeBuilding | Less |
|---|---|---|
| EPDM | 25-30 | 30 to 50 |
| GRP | 25-30 | 25 to 40 |
| Felt | 10-15 | 10 to 20 |
Less adds conditions to its GRP and felt figures. Less says GRP fibreglass lasts 25 to 40 years "with minimal maintenance", and that torch-on felt lasts 10 to 20 years "depending on quality and installation". For EPDM, Less says the rubber membrane "typically lasts 30 to 50 years".
Neither source speaks for any one roof. How long a roof lasts turns on the laying, the drainage, whatever stands on it and the upkeep it gets afterwards. The page on how long a flat roof lasts covers the ground in more depth, and a survey of the roof in front of you is worth more than any table of ranges.
What the garage prices from Which? show
Which? Trusted Traders publish prices for covering a garage, 6m x 3m, drawn from a survey of 11 traders in November 2025. The prices include labour and materials but exclude VAT. A felt roof comes at £1,400 to £3,500 on that garage. A PVC or rubber EPDM roof laid with new boards costs £1,950 to £4,000, on the same garage.
A garage is a small, simple roof, and the figures say nothing about a larger or more complicated one. They indicate a scale, not a quote, and the width of each range shows how much depends on the job: the deck's condition, the access, how many details there are and how thick the covering is.
MyJobQuote gives a separate figure for rubber roofing, putting the average rubber roof at £1,050 fully installed on its page of 9 October 2026, with rubber roofing prices of around £60 per square metre. Those come from another source with other assumptions, and they are not joined to the Which? range.
Our own quote is not a range. It is written out as one total once the survey is done, and its size is set by the roof's area, the covering picked, the deck beneath, the way up to it and the details at the edges. The flat roof replacement costs page sets out the cost picture in more depth.
Falls, Part L and how the choice gets made
Whichever covering is chosen, the roof needs a fall to drain. NFRC says BS 6229:2025 sets "a minimum 1:80 finished fall for general roof areas and internal gutters", while IKO has: "To achieve a 1:80 fall, the code of practice says that the roof should be designed for a fall of 1:40", so tapered insulation is one way to build the slope in. BS 6229:2025 covers continuously supported flexible membranes, and the old 2018 edition has been withdrawn.
Insulation rules come into play on a re-cover. Approved Document L lists a new waterproof layer on a flat roof among its renovation work. Once more than half of the roof surface is involved, the complete roof should be improved to the Table 4.3 standard wherever that proves feasible, and the survey sets out where this lands. The flat roof Building Regulations page sets out the detail.
The survey brings these threads together. The surveyor looks at the deck, the fall, the outlets, the details, the insulation and any rooflights or plant, and reports what the roof showed along with anything else noticed there. A roof with sound boards and easy access may suit any of the three coverings. A roof with a poor deck or an awkward shape narrows the choice.