Lead flashing splits because lead expands and contracts with the weather, and a piece that is too long or fixed too rigidly cannot take that movement, so it cracks along the line of greatest stress.

Get a written quote

Call 01582 935272WhatsApp us

A valley between two concrete tile slopes with a dry valley trough
PicturedA valley between two concrete tile slopes with a dry valley trough.

The short answer

Lead flashing can split because the metal expands when warm and contracts when cold, and a piece that is too long, pinned down too firmly or folded too tightly cannot absorb that movement. Repeated cycles then crack it, along a fold or at a fixing. The specification for a job sets how long each piece runs.

A roof drawing with its parts named: lead valley, tiles, hipLead valleyTilesHip

How movement cracks lead

Lead is a metal, and a metal changes size with temperature. On a warm day a length of flashing grows a little. On a cold night it shrinks back. A strip laid loose enough to slide, held only along its upper edge, takes that in its stride season after season. A strip that is held at several points along its length cannot slide, so the movement has to go somewhere, and it goes into the lead as stress.

Stress that is applied again and again can open a crack, even though no single swing in temperature is large. Cracks can start at the places where the lead is already working hardest: along a fold, at the head of a long piece, beside a nail or screw that holds it down, and where it has been bent sharply or worked more than once. The crack may be fine and hard to see at first, and it widens as the movement continues.

Lead on a slope can also creep, which means it slowly slips downhill under its own weight and thins near the top. A flashing that has crept may split where it has been stretched. The lead roofing hub explains the details where this matters, from walls to valleys.

Causes of a split and what each looks like

A piece too long, a fixing too rigid, sharp or repeated folds, and foot traffic or impact are the causes a survey looks for, and each leaves its own form of split. Several can be present on the same roof.

Causes of split lead flashing
CauseWhat it can look like
Piece too longA crack across the width, near the top
Fixed too rigidlySplits at fixings, with nail heads showing
Sharp or repeated foldsA line crack along the crease
Foot traffic or impactA dent, then a tear on the dent

How long a piece may run is a matter for the specification, which takes the detail and the code of the lead into account, and no single length suits every roof. A roofer who has to make a long run is expected to break it into lapped lengths with room to move, not to lay one long piece. Rolled lead sheet is made to BS EN 12588 in codes 3 to 8, and code 4, for example, is 1.80 mm thick; the code is part of the same specification.

A split caused by a person walking on the lead is separate from one caused by the weather, and the repair is the same in form but not in cause. A ladder resting on a flashing, or a boot on a valley, can dent the lead, and a dent in a fold is a place for a later crack.

What to do about a split flashing

A split in lead flashing lets water behind the covering, so it is worth looking at before the next spell of rain. From the ground, binoculars on a dry day can show a bright line where the metal has opened. Indoors, look for staining on the ceiling or the wall near the flashing, and in the loft for wet timber once rain has stopped. Photograph whatever you find.

Whether the flashing is repaired or replaced depends on the lead around the split. A narrow crack in otherwise sound lead can be repaired, whereas widespread cracking, thinning or lifting points to a new piece, cut so the cause is removed and not copied. The guide to repairing or replacing lead flashing sets that decision out.

A bead of sealant over a split can hide the crack and does nothing about the movement that opened it, so the crack can return beside the sealant. MyJobQuote says correctly installed lead flashing can last for over 80 years, and the guide to signs of failed leadwork explains what to look for on a roof that is not reaching that.

Split lead, questions answered

01Can brand new lead flashing split?

It can, if the piece was laid too long, held too firmly or folded too tightly, because the weather's movement acts on it from the first season. Lead that was formed with room to slide does not meet the same stress. A split in new work points to the specification or the fitting, and it should be raised with whoever laid it, with dated photographs of the split.

02Does frost split lead flashing?

The cold itself does not shatter lead the way it can crack brittle materials. What a cold spell does is shrink the metal, and if the flashing is pinned along its length, it cannot shrink freely. The stress comes from the restraint, not the frost. A flashing that is free to slide at its lower edge copes with the same winter without harm.

03Does a split mean the whole flashing is finished?

Not necessarily. A crack at one fold, in lead that is otherwise firm and flat, may be repaired. A crack that comes with thinning, a creeping top edge or splits along other folds suggests the lead as a whole is tired. The condition of the rest of the piece is what decides, and a survey reads it from close up.

04Will mastic stop a split in lead flashing?

Sealant can slow water for a while, but the lead goes on moving beneath it, and the bead can peel or crack as it does. A roof that leaks through a split and is sealed over may then hide a continuing problem. If water is getting in, photograph the split and the staining inside before any sealant is applied, so that the original fault is documented.