The short answer
Cut-edge corrosion is rust that begins at the cut ends of coated steel roof sheets, where the metal core is exposed. From the edge it can creep beneath the coating and lift it from the surface. Treatment can slow it where the metal is still sound, but sheets that have lost their strength need replacing.
Where the rust begins
A coated steel sheet is made in layers. A steel core carries the load, a metallic layer protects it, and one or more coatings sit on the outside, with a colour on top. All of those layers cover the faces of the sheet. When the sheet is trimmed to fit around a rooflight or meet a ridge, the saw or shear exposes the edge, where the steel and its layers show in section. That bare edge has less protection than the face.
Rain reaches the exposed edge, and rust can take hold. From the edge the corrosion can travel inwards beneath the coating, a process called creep, and the coating lifts in a line of blisters or flakes. The affected zone widens along the cut, so the damage can appear as a thin brown stain along a lap, an end or a hole cut for a pipe.
Edges are not confined to the ends of sheets. They are formed wherever the sheet is cut or drilled: around fixings, at the cut-outs for rooflights and vents, at the notches for flashings and along sheets that were trimmed on site. Every one of those edges can be a starting point, and a roof with many cuts has many places for corrosion to begin. A sheet cut cleanly in a factory can be better protected than one trimmed by hand on the roof.
How far it spreads
Water collects at the laps between sheets, where two cut edges sit one over the other, and an edge there stays damp for longer than an open face. Corrosion at a lap can therefore be well advanced by the time the damage is visible from the ground. The side of a sheet that faces the gutter is another place where water lingers and where the coating can fail.
| Stage | What shows | What it means |
|---|---|---|
| Early | Brown line on the edge | Steel is exposed |
| Spreading | Blistered coating | Rust under the surface |
| Advanced | Flaking, holes | Steel has lost section |
The speed of spread depends on the coating, the amount of moisture, the pollution in the air and whether the roof drains freely. Damp vegetation against a wall, a vent that releases fumes or a roof that holds water in hollows can each make the damage worse. No single timetable fits every roof, which is why the state of the sheets is read in place.
Corrosion in one place may also say something about the whole roof. If the coating is failing across the field of the sheets as well as at the edges, the position differs from a roof where only the laps are affected. The signs of commercial roof failure page lists the wider pattern.
Treatment or replacement
Where the steel is still sound, the rust can be brushed back to clean metal and the edge sealed with a paint or coating system made for the purpose. That may slow the process and gain some extra service from the sheets. It is maintenance and not a cure, and it has to be repeated if the underlying cause stays, for instance a lap that keeps holding water.
Where the metal has thinned, or the corrosion has reached the fixings and the structure, treatment is no longer enough. Holes in the sheets mean the roof leaks, and weakened sheets may not carry loads. Replacement of the damaged sheets, or an overcladding scheme that covers the old sheets with a new system, is then the choice, and the roof overcladding page explains that option.
Corroded sheets can be fragile as well, and on an older building the sheets beneath may be asbestos cement, a question that the asbestos cement roof page takes up. The commercial roofing hub gathers the wider commercial guides, and a figure for the work follows the survey. Staining that runs down from the laps is worth photographing from the ground, to show how fast it moves.